INDUSTRIAL WATER TREATMENT ›› 2003, Vol. 23 ›› Issue (4): 38-41. doi: 10.11894/1005-829x.2003.23(4).38

Previous Articles     Next Articles

Synthesis and performance test of cationic polyacrylamide by copolymerization

Li Zhenghui, Guo Yanli   

  1. Department of applied Chemistry, Natural Science College, Beijing University of Chemical Engineering, Beijing 100029, China
  • Received:2002-08-08 Online:2003-04-20 Published:2010-10-01

共聚合阳离子聚丙烯酰胺的合成及性能测试

李正惠, 郭艳丽   

  1. 北京化工大学理学院应用化学系, 北京 100029
  • 作者简介:李正惠(1941- ), 1965 年毕业于北京化工大学, 副教授。电话:010-64933485

Abstract:

N -(dimethylaminon)methyl acrylamides is synthesized first.Then hydroxymethyl dimethylammonia is synthesized with cationic polyacrylamide by copolymerization.When formaldehyde dimethylamine(mol ratio) is 2 1,the reaction temperature is 55 ℃and the reaction time is 2 h, the yield of hydroxymethyl dimethylammonia is the highest.Acrylamide/cationic acrylamide (mol ratio), temperature and the quantity of redox catalyst have influence on the copolymerization are studied by doing orthogonal test.The results indicate that when acrylamide/cationic acrylamide(mol ratio)is 10 1, the temperature is 45 ℃, the quantity of redox catalyst is 0.04%(the quantity of redox/the total quantity of monomer),the effect is the best.Certain flocculating effect is gained.

Key words: aqueous solution copolymerization, polyacrylamide, copolymerization, flocculant

摘要:

首先合成阳离子单体N-(二甲氨基)甲基丙烯酰胺,然后用共聚合法合成阳离子聚丙烯酰胺。单体合成中探讨了羟甲基二甲胺的合成工艺,当n(甲醛):n(二甲胺)=2:1,反应温度为55℃,反应时间为2h时,羟甲基二甲胺的收率最高;并通过NMR确定了其结构。采用正交实验,研究了共聚合反应中n(丙烯酰胺):n(阳离子丙烯酰胺)、温度、引发剂用量对聚合反应的影响。研究结果表明,n(丙烯酰胺):n(阳离子丙烯酰胺)=10:1,温度为45℃,引发剂质量分数为0.04%时,效果最佳,达到了一定的絮凝效果。

关键词: 水溶液共聚合, 聚丙烯酰胺, 共聚合, 絮凝剂