慈竹高得率制浆废水好氧降解性能研究
盘爱享, 房桂干, 田庆文, 刘行健, 尹航, 杨强, 韩善明

Study on aerobic degradation characteristic of high yield pulping wastewater of Neosinocalamus affinis
Aixiang PAN, Guigan FANG, Qingwen TIAN, Xingjian LIU, Hang YIN, Qiang YANG, Shanming HAN
表1 慈竹高得率制浆工艺条件
Table 1 Technological conditions of high yield pulping of Neosinocalamus affinis
工艺流程项目1#2#3#4#
一段浸渍氢氧化钠/(kg·t-1)20303030
过氧化氢/(kg·t-1)00020
硅酸钠/(kg·t-1)0005
DTPA/(kg·t-1)0002
温度/℃95959595
浆液含固率/%30303030
保温时间/ min45454545
二段浸渍氢氧化钠/(kg·t-1)30304030
过氧化氢/(kg·t-1)00040
硅酸钠/(kg·t-1)00010
DTPA/(kg·t-1)0003
温度/ ℃95~10095~10095~10089
浆液含固率/%30303025
保温时间/ min60606040